Citation
Abstract
The grout under the hydrostatic bearing runner at DSS 14 has exhibited a rapid rate of deterioration and premature failure. This report examines some of the probable causes of the deterioration. It also describes the development of a polymetric grout that is more resistive to the causes of early grout failure.
Details
- Volume
- 42-61
- Published
- February 15, 1981
- Pages
- 115–148
- File Size
- 2.4 MB